EN 10111 Grade StW 22 hot rolled
Equivalent material: AFNOR 1C, BS HR3, UNI FeP11, UNE AP11, ASTM A569, DIN 1.0332, DIN DC11, AFNOR DC11, BS DC11, BS 4CS, BS 4HS, BS 4CR, AISI 1008, SAE 1008, JIS SPHC, JIS SPHD, JIS SEHD, EN DD11, EN 1.0332, ISO HR2, GOST 15kp, ASTM CS Type B
EN 10111 Grade StW 22 hot rolled general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Low Carbon Steel |
EN 10111 Grade StW 22 hot rolled thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K |
Typical for Low Carbon Steel |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Melting point |
- |
Melting point of 1480 - 1526 °C |
Typical for Low Carbon Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 465 J/(kg·K) |
Typical for Low Carbon Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 25 - 93 W/(m·K) |
Typical for Low Carbon Steel |
EN 10111 Grade StW 22 hot rolled chemical
Property |
Value |
Carbon |
Carbon of 0.1 % |
Nitrogen |
Nitrogen of 7E-3 % |
EN 10111 Grade StW 22 hot rolled magnetic
Property |
Value |
Comment |
Curie temperature |
Curie temperature of 770 °C |
Typical for Low Carbon Steel |
EN 10111 Grade StW 22 hot rolled electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m |
Typical for Carbon Steel |
EN 10111 Grade StW 22 hot rolled mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Low Carbon Steel |
Elongation |
20.0 °C |
Elongation of 29 % |
- |
Elongation A80 |
20.0 °C |
Elongation A80 of 25 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Low Carbon Steel |
Shear modulus |
23.0 °C |
Shear modulus of 82 GPa |
Typical for Low Carbon Steel |
Tensile strength |
20.0 °C |
Tensile strength of 440 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 200 MPa |
- |
Lay the foundations of growth and success with our reliable steel materials.
-- Our promise
Similar or equivalent steel materials