ASTM A612 As-Rolled or Normalized and/or Stress Relieved

Equivalent material: DIN 1.8905, DIN StE 460, DIN P460N, BS P460N, JIS SM53B, JIS SM53C, JIS SM520B, JIS SM520C, JIS E460DD, EN P460N, EN 1.8905, ISO E460DD, ASTM F70, ASTM Grade LF6 Class 1, DIN 1.8915, DIN P460NL1, AFNOR P460NL1, BS P460NL1, EN P460NL1, EN 1.8915, ISO P460NL1, DIN 1.8935, DIN WStE 460, DIN P460NH, BS P460NH, EN P460NH, EN 1.8935, ISO P460NH

ASTM A612 As-Rolled or Normalized and/or Stress Relieved general

Property Value Comment
Density Density of 7.8 - 7.9 g/cm³ Typical for Low Carbon Steel

ASTM A612 As-Rolled or Normalized and/or Stress Relieved thermal

Property Value Comment
Coefficient of thermal expansion Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K Typical for Low Carbon Steel
Max service temperature Max service temperature of 291.2 °C Predicted Value, Long
- Max service temperature of 500 °C Typical for Carbon Steel
Melting point Melting point of 1480 - 1526 °C Typical for Low Carbon Steel
Specific heat capacity Specific heat capacity of 465 J/(kg·K) Typical for Low Carbon Steel
Thermal conductivity Thermal conductivity of 25 - 93 W/(m·K) Typical for Low Carbon Steel

ASTM A612 As-Rolled or Normalized and/or Stress Relieved chemical

Property Value Condition Related Standards Shape
Carbon Carbon of 0.25 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate
Chromium Chromium of 0.25 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate
Copper Copper of 0.35 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate
Manganese Manganese of 1 - 1.5 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate
Molybdenum Molybdenum of 0.08 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate
Nickel Nickel of 0.25 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate
Phosphorus Phosphorus of 0.025 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate
Silicon Silicon of 0.15 - 0.5 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate
Sulfur Sulfur of 0.025 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate
Vanadium Vanadium of 0.08 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate

ASTM A612 As-Rolled or Normalized and/or Stress Relieved magnetic

Property Value Comment
Curie temperature Curie temperature of 770 °C Typical for Low Carbon Steel

ASTM A612 As-Rolled or Normalized and/or Stress Relieved electrical

Property Value Comment
Electrical conductivity Electrical conductivity of 7 S/m Predicted Value
Electrical resistivity Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m Typical for Carbon Steel

ASTM A612 As-Rolled or Normalized and/or Stress Relieved mechanical

Property Value Condition Related Standards Shape Comment
Elastic modulus Elastic modulus of 200 - 215 GPa - - - Typical for Low Carbon Steel
Elongation Elongation of 16 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate A200
- Elongation of 17.0 % - - - Predicted Value, A80
- Elongation of 18.5 % - - - Predicted Value, Transverse
- Elongation of 19.3 % - - - Predicted Value, A80 Transverse
- Elongation of 21.9 % - - - Predicted Value
- Elongation of 22 % As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate A50
Poisson's ratio Poisson's ratio of 0.29 [-] - - - Typical for Low Carbon Steel
Reduction of area Reduction of area of 39.7 % - - - Predicted Value
- Reduction of area of 44 % - - - Predicted Value, Transverse
Shear modulus Shear modulus of 82 GPa - - - Typical for Low Carbon Steel
Shear strength Shear strength of 508.2 MPa - - - Predicted Value
Tensile strength Tensile strength of 560 - 695 MPa As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate -
- Tensile strength of 570 - 725 MPa As-Rolled or Normalized and/or Stress Relieved ASTM A612 Plate -