SAE J1268 Grade 5130H
Equivalent material: DIN 1.7030, DIN 28Cr4, AFNOR 28Cr4, BS 28Cr4, AISI 5130H, AISI 5130, SAE 5130, JIS SCr430, JIS SCr430WCH, JIS SCr430H, EN 28Cr4, EN 1.7030, GOST 30Ch, GB/T 30Cr, GB/T A20302, ASTM 5132, UNS H51300, UNS G51300, DIN 1.7036, DIN 28CrS4, AFNOR 28CrS4, BS 28CrS4, EN 28CrS4, EN 1.7036
SAE J1268 Grade 5130H general
| Property |
Temperature |
Value |
Comment |
| Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Steel |
SAE J1268 Grade 5130H thermal
| Property |
Temperature |
Value |
Comment |
| Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 9.4E-6 - 1.5E-5 1/K |
Typical for Chromium Steel |
| Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Steel |
| Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 - 494 J/(kg·K) |
Typical for Chromium Steel |
| Thermal conductivity |
23.0 °C |
Thermal conductivity of 23 - 50 W/(m·K) |
Typical for Chromium Steel |
SAE J1268 Grade 5130H chemical
| Property |
Value |
| Carbon |
Carbon of 0.27 - 0.33 % |
| Chromium |
Chromium of 0.75 - 1.2 % |
| Copper |
Copper of 0.35 % |
| Iron |
balance |
| Manganese |
Manganese of 0.6 - 1 % |
| Silicon |
Silicon of 0.15 - 0.35 % |
SAE J1268 Grade 5130H mechanical
| Property |
Temperature |
Value |
Comment |
| Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Steel |
| Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Steel |