JIS G4307 Grade SUS329J1 cold-rolled, solution annealed

Equivalent material: GB/T 0Cr26Ni5Mo2, GB 0Cr26Ni5Mo2, NF Z3CND25-07Az, NF Z5CND27-05Az, EN X3CrNiMoN27-5-2, UNE X8CrNiMo266, SIS 2324, ASME 329, ASTM S32900, ASTM 329, JIS SUS329J2L, JIS SCS11, JIS SCH11, AISI 329, SAE 329, JIS SUS329J1, UNS S32900

JIS G4307 Grade SUS329J1 cold-rolled, solution annealed general

Property Temperature Value Comment
Density 20.0 °C Density of 7.8 g/cm³ Typical for Duplex Stainless Steel

JIS G4307 Grade SUS329J1 cold-rolled, solution annealed thermal

Property Temperature Value Comment
Coefficient of thermal expansion 20.0 °C Coefficient of thermal expansion of 1E-5 1/K Typical for Duplex Stainless Steel
Max service temperature - Max service temperature of 300 °C Typical for Duplex Stainless Steel
Melting point - Melting point of 1375 - 1450 °C Typical for Duplex Stainless Steel
Specific heat capacity 20.0 °C Specific heat capacity of 440 - 502 J/(kg·K) Typical for Duplex Stainless Steel
Thermal conductivity 20.0 °C Thermal conductivity of 13 - 30 W/(m·K) Typical for Duplex Stainless Steel

JIS G4307 Grade SUS329J1 cold-rolled, solution annealed chemical

Property Value
Carbon Carbon of 0.08 %
Chromium Chromium of 23 - 28 %
Iron Iron of 60.35 - 73 %
Manganese Manganese of 1.5 %
Molybdenum Molybdenum of 1 - 3 %
Nickel Nickel of 3 - 6 %
Phosphorus Phosphorus of 0.04 %
Silicon Silicon of 1 %
Sulfur Sulfur of 0.03 %

JIS G4307 Grade SUS329J1 cold-rolled, solution annealed mechanical

Property Temperature Value Comment
Elastic modulus 20.0 °C Elastic modulus of 200 GPa Typical for Duplex Stainless Steel
Elongation 20.0 °C Elongation of 18 % -
Poisson's ratio 20.0 °C Poisson's ratio of 0.3 [-] Typical for Duplex Stainless Steel
Tensile strength 20.0 °C Tensile strength of 588 MPa -
Yield strength 20.0 °C Yield strength of 392 MPa -

Collaborate with us to bring your vision to life using our premium-grade steel materials.