JIS G4304 Grade SUS317J1 solution treated

Equivalent material: DIN 1.4439, DIN G-X3CrNiMoN17-13-5, DIN X2CrNiMoN17-13-5, AFNOR Z3CND18-14-05Az, UNE F.3544, AISI 317LMN, SAE 317LMN, EN X2CrNiMoN17-13-5, EN 1.4439, ASTM 317LMN, ASTM Grade F48, UNS S31726

JIS G4304 Grade SUS317J1 solution treated general

Property Temperature Value Comment
Density 23.0 °C Density of 7.9 - 8.2 g/cm³ Typical for Austenitic Stainless Steel

JIS G4304 Grade SUS317J1 solution treated thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K Typical for Austenitic Stainless Steel
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 J/(kg·K) Typical for Austenitic Stainless Steel
Thermal conductivity 23.0 °C Thermal conductivity of 11 - 21 W/(m·K) Typical for Austenitic Stainless Steel

JIS G4304 Grade SUS317J1 solution treated electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

JIS G4304 Grade SUS317J1 solution treated mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 195 GPa Typical for Austenitic Stainless Steel
Elongation A5 23.0 °C Elongation A5 of 40 % -
Hardness, Brinell 23.0 °C Hardness, Brinell of 187 [-] -
Hardness, Rockwell B 23.0 °C Hardness, Rockwell B of 90 [-] -
Hardness, Vickers 23.0 °C Hardness, Vickers of 200 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 480 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 175 MPa -