Property |
Temperature |
Value |
Density |
20.0 °C |
Density of 7.85 g/cm³ |
EN 10277-5 Grade Cm60 cold drawn thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
100.0 °C |
Coefficient of thermal expansion of 1.11E-5 1/K |
- |
- |
200.0 °C |
Coefficient of thermal expansion of 1.21E-5 1/K |
- |
- |
300.0 °C |
Coefficient of thermal expansion of 1.29E-5 1/K |
- |
- |
400.0 °C |
Coefficient of thermal expansion of 1.35E-5 1/K |
- |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Max service temperature, long |
- |
Max service temperature, long of -25 - 0 °C |
- |
Melting point |
- |
Melting point of 1289 - 1478 °C |
Typical for High Carbon Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 486 J/(kg·K) |
Typical for High Carbon Steel |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 51 W/(m·K) |
- |
- |
100.0 °C |
Thermal conductivity of 49.9 W/(m·K) |
- |
- |
200.0 °C |
Thermal conductivity of 47.8 W/(m·K) |
- |
- |
300.0 °C |
Thermal conductivity of 44.8 W/(m·K) |
- |
EN 10277-5 Grade Cm60 cold drawn chemical
Property |
Value |
Carbon |
Carbon of 0.57 - 0.65 % |
Manganese |
Manganese of 0.6 - 0.9 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.4 % |
Sulfur |
Sulfur of 0.02 - 0.035 % |
EN 10277-5 Grade Cm60 cold drawn electrical
Property |
Temperature |
Value |
Electrical resistivity |
20.0 °C |
Electrical resistivity of 1.3E-7 Ω·m |
EN 10277-5 Grade Cm60 cold drawn mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
20.0 °C |
Elastic modulus of 210 GPa |
- |
- |
100.0 °C |
Elastic modulus of 205 GPa |
- |
- |
200.0 °C |
Elastic modulus of 195 GPa |
- |
- |
300.0 °C |
Elastic modulus of 185 GPa |
- |
- |
400.0 °C |
Elastic modulus of 175 GPa |
- |
Elongation |
20.0 °C |
Elongation of 4 - 8 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for High Carbon Steel |
Shear modulus |
20.0 °C |
Shear modulus of 81 GPa |
- |
Tensile strength |
20.0 °C |
Tensile strength of 670 - 860 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 380 - 700 MPa |
- |