ASTM A403 Grade S32053 Heat-Treated

Equivalent material: JIS SUS836L, ASTM F70, UNS S32053

ASTM A403 Grade S32053 Heat-Treated general

Property Temperature Value Comment
Density 23.0 °C Density of 8.8 g/cm³ Typical for Nickel Steel

ASTM A403 Grade S32053 Heat-Treated thermal

Property Temperature Value Comment
Melting point - Melting point of 1316 - 1595 °C Typical for Nickel Steel
Specific heat capacity 23.0 °C Specific heat capacity of 456 J/(kg·K) Typical for Nickel Steel
Thermal conductivity 23.0 °C Thermal conductivity of 10 - 50 W/(m·K) Typical for Nickel Steel

ASTM A403 Grade S32053 Heat-Treated chemical

Property Value
Carbon Carbon of 0.03 %
Chromium Chromium of 22 - 24 %
Manganese Manganese of 1 %
Molybdenum Molybdenum of 5 - 6 %
Nickel Nickel of 24 - 26 %
Nitrogen Nitrogen of 0.17 - 0.22 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 1 %
Sulfur Sulfur of 0.01 %

ASTM A403 Grade S32053 Heat-Treated mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Nickel Steel
Elongation A50 23.0 °C Elongation A50 of 20 - 28 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Steel
Shear modulus 23.0 °C Shear modulus of 76 GPa Typical for Nickel Steel
Tensile strength 23.0 °C Tensile strength of 640 MPa -
Yield strength 23.0 °C Yield strength of 295 MPa -