ASTM A336 Grade F1 Annealed or Normalized and Tempered

Equivalent material: DIN 1.5415, DIN 15Mo3, DIN 16Mo3, AFNOR 16Mo3, AFNOR 15D3, BS 16Mo3, JIS STBA12, JIS STPA12, JIS STFA12, EN 16Mo3, EN 1.5415, ISO 16Mo3, ISO F26, DIN 1.5421, DIN 20MnMo3-5, EN 1.5421, UNS K12822, DIN 1.5423, DIN 16Mo5, BS 1503-245-420, UNI 16Mo5, UNE 16Mo5, AISI 4520, SAE 4520, JIS SB450M, JIS SB480, JIS SB480M, JIS STBA13, JIS SB49M, EN 1.5423, ASTM Grade T1

ASTM A336 Grade F1 Annealed or Normalized and Tempered general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Molybdenum Steel

ASTM A336 Grade F1 Annealed or Normalized and Tempered thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.29E-5 1/K Typical for Molybdenum Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Molybdenum Steel
Specific heat capacity 23.0 °C Specific heat capacity of 456 J/(kg·K) Typical for Molybdenum Steel
Thermal conductivity 23.0 °C Thermal conductivity of 37 - 48 W/(m·K) Typical for Molybdenum Steel

ASTM A336 Grade F1 Annealed or Normalized and Tempered chemical

Property Value
Carbon Carbon of 0.2 - 0.3 %
Manganese Manganese of 0.6 - 0.8 %
Molybdenum Molybdenum of 0.4 - 0.6 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 0.2 - 0.35 %
Sulfur Sulfur of 0.025 %

ASTM A336 Grade F1 Annealed or Normalized and Tempered mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Molybdenum Steel
Elongation A50 23.0 °C Elongation A50 of 20 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Molybdenum Steel
Reduction of area 23.0 °C Reduction of area of 40 % -
Tensile strength 23.0 °C Tensile strength of 485 - 660 MPa -
Yield strength 23.0 °C Yield strength of 275 MPa -