AISI 420 Hardened

Equivalent material: DIN 1.4021, DIN X20Cr13, DIN X30Cr13, AFNOR Z20C13, BS 420S37, BS 420S29, UNI X20Cr13, SS 2303, SAE 420, JIS SUS420J1, JIS SUS 420J1, JIS SUS420J1FB, JIS SUS420J1TKA, EN X20Cr13, EN 1.4021, ISO 20Cr13, GOST 20Ch13, GB 2Cr13, UNS S42000, DIN 1.4031, BS 420S45, SS 2304, EN X39Cr13, EN 1.4031, DIN 1.4034, DIN X46Cr13, AFNOR Z44C14, UNI X40Cr14, UNE F.3405, EN X46Cr13, EN 1.4034, ISO X46Cr13, GOST 40Ch13

AISI 420 Hardened general

Property Temperature Value
Density 23.0 °C Density of 7.8 g/cm³

AISI 420 Hardened thermal

Property Temperature Value
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1E-5 1/K
Melting point - Melting point of 1450 °C
Specific heat capacity 23.0 °C Specific heat capacity of 460 J/(kg·K)
Thermal conductivity 23.0 °C Thermal conductivity of 30 W/(m·K)

AISI 420 Hardened chemical

Property Value
Carbon Carbon of 0.15 - 0.4 %
Chromium Chromium of 12 - 14 %
Iron Iron of 82.3 - 87.9 %
Manganese Manganese of 0 - 1.5 %
Molybdenum Molybdenum of 0 - 0.5 %
Nickel Nickel of 0 - 0.75 %
Phosphorus Phosphorus of 0 - 0.04 %
Silicon Silicon of 0 - 1 %
Sulfur Sulfur of 0 - 0.03 %

AISI 420 Hardened electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 6E-7 Ω·m Typical for Martensitic Stainless Steel

AISI 420 Hardened mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 210 GPa -
Elongation 23.0 °C Elongation of 12 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Martensitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Martensitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 980 MPa -
Yield strength 23.0 °C Yield strength of 760 MPa -