AISI 317LMN Annealed

Equivalent material: DIN 1.4439, DIN G-X3CrNiMoN17-13-5, DIN X2CrNiMoN17-13-5, AFNOR Z3CND18-14-05Az, UNE F.3544, SAE 317LMN, JIS SUS317J1, EN X2CrNiMoN17-13-5, EN 1.4439, ASTM 317LMN, ASTM Grade F48, UNS S31726

AISI 317LMN Annealed general

Property Temperature Value
Density 23.0 °C Density of 8 g/cm³

AISI 317LMN Annealed thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.3E-5 1/K -
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 500 J/(kg·K) -
Thermal conductivity 23.0 °C Thermal conductivity of 14 W/(m·K) -

AISI 317LMN Annealed chemical

Property Value
Carbon Carbon of 0 - 0.03 %
Chromium Chromium of 16.5 - 20 %
Iron Iron of 54.4 - 66.9 %
Manganese Manganese of 0 - 2 %
Molybdenum Molybdenum of 4 - 5 %
Nickel Nickel of 12.5 - 17.5 %
Nitrogen Nitrogen of 0.1 - 0.22 %
Phosphorus Phosphorus of 0 - 0.05 %
Silicon Silicon of 0 - 1 %
Sulfur Sulfur of 0 - 0.03 %

AISI 317LMN Annealed electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

AISI 317LMN Annealed mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 GPa -
Elongation 23.0 °C Elongation of 46 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 630 MPa -
Yield strength 23.0 °C Yield strength of 280 MPa -