AISI 202 Annealed
Equivalent material: DIN 1.4373, BS 284S16, SAE 202, JIS SUS202, EN X12CrMnNiN18-9-5, EN 1.4373, GOST 12X17 9AH4, UNS S20200, ASTM TP202, ASTM 202
AISI 202 Annealed general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 7.7 g/cm³ |
AISI 202 Annealed thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
- |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 500 J/(kg·K) |
- |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 15 W/(m·K) |
- |
AISI 202 Annealed chemical
Property |
Value |
Carbon |
Carbon of 0 - 0.15 % |
Chromium |
Chromium of 17 - 19 % |
Iron |
Iron of 63 - 71.5 % |
Manganese |
Manganese of 7.5 - 10.5 % |
Nickel |
Nickel of 4 - 6 % |
Nitrogen |
Nitrogen of 0 - 0.25 % |
Phosphorus |
Phosphorus of 0 - 0.06 % |
Silicon |
Silicon of 0 - 1 % |
Sulfur |
Sulfur of 0 - 0.03 % |
AISI 202 Annealed electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
AISI 202 Annealed mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 GPa |
- |
Elongation |
23.0 °C |
Elongation of 46 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 710 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 320 MPa |
- |