AISI 201L 1/8-Hard
Equivalent material: DIN 1.4371, DIN X2CrMnNiN17-7-5, AFNOR X2CrMnNiN17-7-5, BS X2CrMnNiN17-7-5, AISI S20103, AISI 201LN, AISI S20153, SAE S20103, SAE 201LN, SAE 201L, SAE S20153, JIS SUS202, EN X2CrMnNiN17-7-5, EN 1.4371, ASTM TP201LN, UNS S20153, UNS S20103
AISI 201L 1/8-Hard general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 7.7 g/cm³ |
AISI 201L 1/8-Hard thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
- |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 450 J/(kg·K) |
- |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
AISI 201L 1/8-Hard chemical
Property |
Value |
Carbon |
Carbon of 0 - 0.03 % |
Chromium |
Chromium of 16 - 18 % |
Iron |
Iron of 67.9 - 75 % |
Manganese |
Manganese of 5.5 - 7.5 % |
Nickel |
Nickel of 3.5 - 5.5 % |
Nitrogen |
Nitrogen of 0 - 0.25 % |
Phosphorus |
Phosphorus of 0 - 0.05 % |
Silicon |
Silicon of 0 - 0.75 % |
Sulfur |
Sulfur of 0 - 0.03 % |
AISI 201L 1/8-Hard electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
AISI 201L 1/8-Hard mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 220 GPa |
- |
Elongation |
23.0 °C |
Elongation of 40 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 830 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 440 MPa |
- |