UNS S20910 Strain Hardened

Equivalent material: ASTM TPXM-19, ASTM XM-19, ASTM S20910, ASTM Grade FXM-19, ASTM FXM-19, ASTM Grade 8R, AISI XM-19, SAE XM-19, ASTM Grade B8R, ASTM Grade B8RA, ASTM Grade 8RA

UNS S20910 Strain Hardened general

Property Temperature Value
Density 23.0 °C Density of 7.8 g/cm³

UNS S20910 Strain Hardened thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.6E-5 1/K -
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 480 J/(kg·K) -
Thermal conductivity 23.0 °C Thermal conductivity of 13 W/(m·K) -

UNS S20910 Strain Hardened chemical

Property Value
Carbon Carbon of 0 - 0.06 %
Chromium Chromium of 20.5 - 23.5 %
Iron Iron of 52.1 - 62.1 %
Manganese Manganese of 4 - 6 %
Molybdenum Molybdenum of 1.5 - 3 %
Nickel Nickel of 11.5 - 13.5 %
Niobium Niobium of 0.1 - 0.3 %
Nitrogen Nitrogen of 0.2 - 0.4 %
Phosphorus Phosphorus of 0 - 0.04 %
Silicon Silicon of 0 - 0.75 %
Sulfur Sulfur of 0 - 0.03 %
Vanadium Vanadium of 0.1 - 0.3 %

UNS S20910 Strain Hardened electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

UNS S20910 Strain Hardened mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 220 GPa -
Elongation 23.0 °C Elongation of 14 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 950 MPa -
Yield strength 23.0 °C Yield strength of 830 MPa -