SAE J405 Grade 439
Equivalent material: DIN 1.4510, DIN X3CrTi17, DIN GX40CrSi29, DIN X6CrTi17, AISI 439, JIS SUS430LX, JIS SUS430LXTP, JIS SUS430LXTB, JIS SUSXM8TB, EN X3CrTi17, EN 1.4510, UNS S43036, ASTM TP439, ASTM 439, UNS S43035
SAE J405 Grade 439 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.6 - 7.8 g/cm³ |
Typical for Ferritic Stainless Steel |
SAE J405 Grade 439 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 9.3E-6 - 1.2E-5 1/K |
Typical for Ferritic Stainless Steel |
Melting point |
- |
Melting point of 1425 - 1530 °C |
Typical for Ferritic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 420 - 586 J/(kg·K) |
Typical for Ferritic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 22 W/(m·K) |
Typical for Ferritic Stainless Steel |
SAE J405 Grade 439 chemical
Property |
Value |
Aluminium |
Aluminium of 0.15 % |
Carbon |
Carbon of 0.07 % |
Chromium |
Chromium of 17 - 19 % |
Manganese |
Manganese of 1 % |
Nickel |
Nickel of 0.5 % |
Nitrogen |
Nitrogen of 0.04 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 1 % |
Sulfur |
Sulfur of 0.03 % |
SAE J405 Grade 439 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 6E-7 - 7.5E-7 Ω·m |
Typical for Ferritic Stainless Steel |
SAE J405 Grade 439 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 220 GPa |
Typical for Ferritic Stainless Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Ferritic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Ferritic Stainless Steel |