SAE J405 Grade 430
Equivalent material: DIN 1.4016, DIN X6Cr17, DIN X8Cr17, DIN X3CrTi17, AFNOR Z8C17, BS 430S15, UNI X8Cr17, SS 2320, UNE F.3113, AISI 430, JIS SUS430, JIS SUS430TP, JIS SUS430TB, JIS SUS430TKA, JIS SUS430TKC, JIS SUSY430, EN X6Cr17, EN 1.4016, ISO X6Cr17, ISO F1, GOST 12Ch17, GB 1Cr17, ASTM S43000, UNS S43000, ASTM MT430, ASTM 430, ASTM TP430, ASTM F430
SAE J405 Grade 430 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.6 - 7.8 g/cm³ |
Typical for Ferritic Stainless Steel |
SAE J405 Grade 430 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 9.3E-6 - 1.2E-5 1/K |
Typical for Ferritic Stainless Steel |
Melting point |
- |
Melting point of 1425 - 1530 °C |
Typical for Ferritic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 420 - 586 J/(kg·K) |
Typical for Ferritic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 22 W/(m·K) |
Typical for Ferritic Stainless Steel |
SAE J405 Grade 430 chemical
Property |
Value |
Carbon |
Carbon of 0.12 % |
Chromium |
Chromium of 16 - 18 % |
Manganese |
Manganese of 1 % |
Nickel |
Nickel of 0.75 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 1 % |
Sulfur |
Sulfur of 0.03 % |
SAE J405 Grade 430 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 6E-7 - 7.5E-7 Ω·m |
Typical for Ferritic Stainless Steel |
SAE J405 Grade 430 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 220 GPa |
Typical for Ferritic Stainless Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Ferritic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Ferritic Stainless Steel |