JIS G4314 Grade SUS302

Equivalent material: GB 1Cr18Ni9, GB/T 1Cr18Ni9, GB/T 1Cr18Ni9-L, GB/T 1Cr18Ni9-Q, GB/T 1Cr18Ni9-R, GB 1Cr18Ni9, GB 1Cr19Ni9, AISI 302, SAE 302, ASTM MT302, ASTM 302, UNS S30200, DIN 1.4325, DIN X9CrNi18-9, JIS SUS303Se, EN 1.4325, UNS 30302

JIS G4314 Grade SUS302 general

Property Temperature Value Comment
Density 23.0 °C Density of 7.9 - 8.2 g/cm³ Typical for Austenitic Stainless Steel

JIS G4314 Grade SUS302 thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K Typical for Austenitic Stainless Steel
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 J/(kg·K) Typical for Austenitic Stainless Steel
Thermal conductivity 23.0 °C Thermal conductivity of 11 - 21 W/(m·K) Typical for Austenitic Stainless Steel

JIS G4314 Grade SUS302 electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

JIS G4314 Grade SUS302 mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 195 GPa Typical for Austenitic Stainless Steel
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 880 - 2400 MPa -