JIS G4309 Grade SUS310S
Equivalent material: GB H1Cr26Ni21, GOST 20Х23Н18, GOST 20H23N18, DIN X12CrNi2520, DIN 2520, NF Z12CN25-20, NF Z8CN25-20, NF Z12CN26-21, BS 310S16, BS 310S94, BS 313S94, BS 310S24, UNI X6CrNi2520, UNI X6CrNi2521KG, UNI X6CrNi2521KW, UNE F.331, SIS 2361, AMS 5521, AMS 5572, AMS 5577, AMS 5651, AMS 7490, ASME 310S, ASTM TP310S, ASTM 310S, ASTM MT310S, JIS SUSY310S, AISI 310S, ASTM CR310S, ASTM WP310S, SAE 310S, ASTM S31008, UNS S31008
JIS G4309 Grade SUS310S general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
JIS G4309 Grade SUS310S thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
JIS G4309 Grade SUS310S electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
JIS G4309 Grade SUS310S mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Elongation A5 |
23.0 °C |
Elongation A5 of 20 - 30 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 500 - 1130 MPa |
- |