JIS G3463 Grade SUSXM8TB
Equivalent material: DIN 1.4510, DIN X3CrTi17, DIN GX40CrSi29, DIN X6CrTi17, AISI 439, SAE 439, JIS SUS430LX, JIS SUS430LXTP, JIS SUS430LXTB, EN X3CrTi17, EN 1.4510, UNS S43036
JIS G3463 Grade SUSXM8TB general
| Property |
Temperature |
Value |
Comment |
| Density |
23.0 °C |
Density of 7.6 - 7.8 g/cm³ |
Typical for Ferritic Stainless Steel |
JIS G3463 Grade SUSXM8TB thermal
| Property |
Temperature |
Value |
Comment |
| Elastic modulus |
23.0 °C |
Elastic modulus of 220 GPa |
Typical for Ferritic Stainless Steel |
| Elongation A5 |
23.0 °C |
Elongation A5 of 11 - 20 % |
- |
| Hardness, Rockwell B |
23.0 °C |
Hardness, Rockwell B of 90 [-] |
- |
| Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Ferritic Stainless Steel |
| Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Ferritic Stainless Steel |
| Tensile strength |
23.0 °C |
Tensile strength of 410 MPa |
- |
| Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 205 MPa |
- |
JIS G3463 Grade SUSXM8TB magnetic
| Property |
Temperature |
Value |
Comment |
| Electrical resistivity |
23.0 °C |
Electrical resistivity of 6E-7 - 7.5E-7 Ω·m |
Typical for Ferritic Stainless Steel |
JIS G3463 Grade SUSXM8TB electrical
| Property |
Temperature |
Value |
Comment |
| Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 9.3E-6 - 1.2E-5 1/K |
Typical for Ferritic Stainless Steel |
| Melting point |
- |
Melting point of 1425 - 1530 °C |
Typical for Ferritic Stainless Steel |
| Specific heat capacity |
23.0 °C |
Specific heat capacity of 420 - 586 J/(kg·K) |
Typical for Ferritic Stainless Steel |
| Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 22 W/(m·K) |
Typical for Ferritic Stainless Steel |
JIS G3463 Grade SUSXM8TB mechanical
| Property |
Value |
| Wall thickness |
Wall thickness of 1 - 8 mm |
Trust our premium-grade steel products to deliver unmatched performance and durability for your projects.
-- Our promise
Similar or equivalent steel materials
Get a quote