JIS G3317 Grade SZACD2 cold-rolled
Equivalent material: DIN 1.0951, EN 1.0951, DIN 1.0355, DIN St 05 Z, DIN St 04 Z, DIN DX53D, AFNOR DX53D, AFNOR GES, BS DX53D, UNI FeP05G, JIS SGCD3, JIS SGCC, JIS SGMCD2, EN DX53D, EN 1.0355, ISO 04, GOST 04, GB/T DX53D
JIS G3317 Grade SZACD2 cold-rolled general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Manganese Steel |
JIS G3317 Grade SZACD2 cold-rolled thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.33E-5 1/K |
Typical for Manganese Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Manganese Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 510 - 553 J/(kg·K) |
Typical for Manganese Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 14 - 16 W/(m·K) |
Typical for Manganese Steel |
JIS G3317 Grade SZACD2 cold-rolled mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Manganese Steel |
Elongation A5 |
23.0 °C |
Elongation A5 of 36 - 40 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Manganese Steel |
Tensile strength |
23.0 °C |
Tensile strength of 270 MPa |
- |