EN 10025-5 Grade S355K2G1W as-rolled condition (+AR)
EN 10025-5 Grade S355K2G1W as-rolled condition (+AR) introduction
The material S355K2G1W with improved atmospheric corrosion resistance (by generation of an conversion coating) has a minimum yield strength of 355 N/mm². It is applicated for welded, screwed and riveted constructions, e.g. structural engineering, bridge building, tank construction, exhaust systems, vehicle construction, toolbuilding.
The atmospheric load have to consider (SEW 087, Guideline 007 of the Deutscher Ausschuss für Stahlbau and paragraph 2.5 of TA-Luft 1986).
The unhindered generation of the conversion coating have to be considered in the construction and building process.
The grid rate have to considered in the dimensioning process. An conventional surface protection is recommend at polluted air and necessary at long-time water wetting, constant wetness or close to the sea. Unweathered areas with condensate generation have to be adequate ventilated.
Before welding the coating have to be removed in a distance of 10 - 20 mm from the welding edge.
With increasing thickness, strength and carbon equivalent the occurence of cold cracks in the welding zone is possible.
The recommendation of the EURONORM Information No. 2 (EN 1011) have to considered.
Application limit: An notch impact energy of 40 J at -20 deg. is guaranteed.
Equivalent material: DIN 1.8966, DIN S355K2G1W, DIN S355K2W, JIS SMA50CW, JIS SMA490CW, EN 1.8966, ASTM Type IV Grade II, ASTM Type IV
EN 10025-5 Grade S355K2G1W as-rolled condition (+AR) general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
Typical for Steel |
EN 10025-5 Grade S355K2G1W as-rolled condition (+AR) chemical
Property |
Value |
Carbon |
Carbon of 0.16 % |
Chromium |
Chromium of 0.4 - 0.8 % |
Copper |
Copper of 0.25 - 0.55 % |
Manganese |
Manganese of 0.5 - 1 % |
Molybdenum |
Molybdenum of 0.3 % |
Nickel |
Nickel of 0.65 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.5 % |
Sulfur |
Sulfur of 0.035 % |
Zirconium |
Zirconium of 0.15 % |
EN 10025-5 Grade S355K2G1W as-rolled condition (+AR) mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 190 - 210 GPa |
Typical for Steel |
Elongation |
20.0 °C |
Elongation of 20 - 22 % |
- |
Elongation A80 |
20.0 °C |
Elongation A80 of 16 - 18 % |
- |
Elongation A80, transverse |
20.0 °C |
Elongation A80, transverse of 14 - 16 % |
- |
Elongation, transverse |
20.0 °C |
Elongation, transverse of 18 - 20 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Steel |
Tensile strength |
20.0 °C |
Tensile strength of 490 - 680 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 315 - 355 MPa |
- |
Get the best value for your money with our top-grade steel at competitive prices.
-- Our promise
Similar or equivalent steel materials
Get a quote