ASTM A744 Grade CF3 Heat-Treated

Equivalent material: DIN 1.4309, BS 304C12, AISI 304L, SAE 304L, JIS SCS13, EN GX2CrNi19-11, EN 1.4309, ASTM Grade CPF3, UNS J92500

ASTM A744 Grade CF3 Heat-Treated general

Property Temperature Value Comment
Density 23.0 °C Density of 7.9 - 8.2 g/cm³ Typical for Austenitic Stainless Steel

ASTM A744 Grade CF3 Heat-Treated thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K Typical for Austenitic Stainless Steel
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 J/(kg·K) Typical for Austenitic Stainless Steel
Thermal conductivity 23.0 °C Thermal conductivity of 11 - 21 W/(m·K) Typical for Austenitic Stainless Steel

ASTM A744 Grade CF3 Heat-Treated chemical

Property Value
Carbon Carbon of 0.03 %
Chromium Chromium of 17 - 21 %
Manganese Manganese of 1.5 %
Nickel Nickel of 8 - 12 %
Phosphorus Phosphorus of 0.04 %
Silicon Silicon of 2 %
Sulfur Sulfur of 0.04 %

ASTM A744 Grade CF3 Heat-Treated electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

ASTM A744 Grade CF3 Heat-Treated mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 195 GPa Typical for Austenitic Stainless Steel
Elongation A50 23.0 °C Elongation A50 of 35 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 485 MPa -
Yield strength 23.0 °C Yield strength of 205 MPa -