ASTM A575 Grade M1017
Equivalent material: DIN 1.0416, DIN C18D, AFNOR C18D, BS C18D, AISI 1017, SAE 1017, JIS SWRM17, JIS S17C, EN C18D, EN 1.0416, ISO C18D, GB/T C18D, GB/T U53182, ASTM Grade 1017, UNS G10170
ASTM A575 Grade M1017 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Low Carbon Steel |
ASTM A575 Grade M1017 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K |
Typical for Low Carbon Steel |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Melting point |
- |
Melting point of 1480 - 1526 °C |
Typical for Low Carbon Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 465 J/(kg·K) |
Typical for Low Carbon Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 25 - 93 W/(m·K) |
Typical for Low Carbon Steel |
ASTM A575 Grade M1017 chemical
Property |
Value |
Carbon |
Carbon of 0.14 - 0.21 % |
Manganese |
Manganese of 0.25 - 0.6 % |
Phosphorus |
Phosphorus of 0.04 % |
Sulfur |
Sulfur of 0.05 % |
ASTM A575 Grade M1017 magnetic
Property |
Value |
Comment |
Curie temperature |
Curie temperature of 770 °C |
Typical for Low Carbon Steel |
ASTM A575 Grade M1017 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m |
Typical for Carbon Steel |
ASTM A575 Grade M1017 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Low Carbon Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Low Carbon Steel |
Shear modulus |
23.0 °C |
Shear modulus of 82 GPa |
Typical for Low Carbon Steel |