ASTM A487 Grade CA15 Class D, Heat-Treated
Equivalent material: DIN 1.4008, EN GX7CrNiMo12-1, EN 1.4008, ASTM CA15, UNS J91150
ASTM A487 Grade CA15 Class D, Heat-Treated general
Property |
Temperature |
Value |
Comment |
Density |
20.0 °C |
Density of 7.6 - 7.7 g/cm³ |
Typical for Martensitic Stainless Steel |
ASTM A487 Grade CA15 Class D, Heat-Treated thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
20.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.5E-5 1/K |
Typical for Martensitic Stainless Steel |
Melting point |
- |
Melting point of 1375 - 1450 °C |
Typical for Martensitic Stainless Steel |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 14 - 31 W/(m·K) |
Typical for Martensitic Stainless Steel |
ASTM A487 Grade CA15 Class D, Heat-Treated chemical
Property |
Value |
Carbon |
Carbon of 0 - 0.15 % |
Copper |
Copper of 0 - 0.1 % |
Manganese |
Manganese of 0 - 1 % |
Molybdenum |
Molybdenum of 0 - 0.5 % |
Nickel |
Nickel of 0 - 0.05 % |
Phosphorus |
Phosphorus of 0 - 0.04 % |
Silicon |
Silicon of 0 - 1.5 % |
Sulfur |
Sulfur of 0 - 0.035 % |
ASTM A487 Grade CA15 Class D, Heat-Treated mechanical
Property |
Temperature |
Value |
Comment |
Elongation A50 |
20.0 °C |
Elongation A50 of 0 - 17 % |
- |
Hardness, Brinell |
20.0 °C |
Hardness, Brinell of 0 - 235 [-] |
- |
Hardness, Rockwell C |
20.0 °C |
Hardness, Rockwell C of 0 - 22 [-] |
- |
Poisson's ratio |
20.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Martensitic Stainless Steel |
Reduction of area |
20.0 °C |
Reduction of area of 0 - 35 % |
- |
Tensile strength |
20.0 °C |
Tensile strength of 0 - 690 MPa |
- |
Yield Strength Rp0.2, short transverse |
20.0 °C |
Yield Strength Rp0.2, short transverse of 0 - 515 MPa |
- |