ASTM A487 Grade 11 Class B, Heat-Treated
Equivalent material: ASTM Grade 11Q, ASTM IC 4620, ASTM Grade 11
ASTM A487 Grade 11 Class B, Heat-Treated general
| Property |
Temperature |
Value |
Comment |
| Density |
20.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Nickel Molybdenum Steel |
ASTM A487 Grade 11 Class B, Heat-Treated thermal
| Property |
Temperature |
Value |
Comment |
| Coefficient of thermal expansion |
20.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
Typical for Nickel Molybdenum Steel 20-300°C |
| Melting point |
- |
Melting point of 1529 °C |
Typical for Nickel Molybdenum Steel |
ASTM A487 Grade 11 Class B, Heat-Treated chemical
| Property |
Value |
| Carbon |
Carbon of 0.05 - 0.2 % |
| Copper |
Copper of 0 - 0.5 % |
| Manganese |
Manganese of 0.5 - 0.8 % |
| Molybdenum |
Molybdenum of 0.45 - 0.65 % |
| Phosphorus |
Phosphorus of 0 - 0.04 % |
| Silicon |
Silicon of 0 - 0.6 % |
| Sulfur |
Sulfur of 0 - 0.035 % |
| Tungsten |
Tungsten of 0 - 0.1 % |
| Vanadium |
Vanadium of 0 - 0.03 % |
ASTM A487 Grade 11 Class B, Heat-Treated mechanical
| Property |
Temperature |
Value |
Comment |
| Elongation A50 |
20.0 °C |
Elongation A50 of 0 - 17 % |
- |
| Poisson's ratio |
20.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Molybdenum Steel |
| Reduction of area |
20.0 °C |
Reduction of area of 0 - 35 % |
- |
| Tensile strength |
20.0 °C |
Tensile strength of 0 - 725 MPa |
- |
| Yield Strength Rp0.2, short transverse |
20.0 °C |
Yield Strength Rp0.2, short transverse of 0 - 585 MPa |
- |
Discover innovative solutions at every stage of your project journey with our steel expertise.