ASTM A333 Grade 11 Heat-Treated

Equivalent material: ASTM Grade 11Q, ASTM IC 4620

ASTM A333 Grade 11 Heat-Treated general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Nickel Molybdenum Steel

ASTM A333 Grade 11 Heat-Treated thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 9E-6 - 1.3E-5 1/K Typical for Nickel Molybdenum Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Nickel Molybdenum Steel
Specific heat capacity 23.0 °C Specific heat capacity of 335 - 481 J/(kg·K) Typical for Nickel Molybdenum Steel
Thermal conductivity 23.0 °C Thermal conductivity of 44 W/(m·K) Typical for Nickel Molybdenum Steel

ASTM A333 Grade 11 Heat-Treated chemical

Property Value
Carbon Carbon of 0.1 %
Chromium Chromium of 0.5 %
Cobalt Cobalt of 0.5 %
Manganese Manganese of 0.6 %
Molybdenum Molybdenum of 0.5 %
Nickel Nickel of 35 - 37 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 0.35 %
Sulfur Sulfur of 0.025 %

ASTM A333 Grade 11 Heat-Treated mechanical

Property Temperature Value Comment
Charpy impact energy 23.0 °C Charpy impact energy of 18 J -
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Nickel Molybdenum Steel
Elongation A50 23.0 °C Elongation A50 of 18 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Molybdenum Steel
Tensile strength 23.0 °C Tensile strength of 450 MPa -
Yield strength 23.0 °C Yield strength of 240 MPa -