ASTM A471 Class 1 Heat-Treated
Equivalent material: ASTM Class 2, ASTM Class 3, ASTM Class 4, ASTM Class 5, ASTM Class 6
ASTM A471 Class 1 Heat-Treated general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
Typical for Steel |
ASTM A471 Class 1 Heat-Treated chemical
Property |
Value |
Aluminium |
Aluminium of 0.015 % |
Carbon |
Carbon of 0.28 % |
Chromium |
Chromium of 0.75 - 2 % |
Manganese |
Manganese of 0.7 % |
Molybdenum |
Molybdenum of 0.2 - 0.7 % |
Nickel |
Nickel of 2 - 4 % |
Phosphorus |
Phosphorus of 0.01 % |
Sulfur |
Sulfur of 0.015 % |
Vanadium |
Vanadium of 0.05 % |
ASTM A471 Class 1 Heat-Treated mechanical
Property |
Temperature |
Value |
Comment |
Charpy impact energy |
23.0 °C |
Charpy impact energy of 68 J |
- |
Elastic modulus |
23.0 °C |
Elastic modulus of 190 - 210 GPa |
Typical for Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 20 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Steel |
Reduction of area |
23.0 °C |
Reduction of area of 50 % |
- |
Tensile strength |
23.0 °C |
Tensile strength of 690 MPa |
- |
Yield strength Rp0.02 |
23.0 °C |
Yield strength Rp0.02 of 520 - 655 MPa |
- |
Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 550 - 690 MPa |
- |
Our steel products inspire endless possibilities while ensuring engineering excellence.
-- Our promise
Similar or equivalent steel materials