ASTM A471 Class 5 Heat-Treated general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Medium Carbon Steel |
ASTM A471 Class 5 Heat-Treated thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.32E-5 1/K |
Typical for Medium Carbon Steel |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Melting point |
- |
Melting point of 1380 - 1514 °C |
Typical for Medium Carbon Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 470 - 520 J/(kg·K) |
Typical for Medium Carbon Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 21 - 52 W/(m·K) |
Typical for Medium Carbon Steel |
ASTM A471 Class 5 Heat-Treated electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m |
Typical for Carbon Steel |
ASTM A471 Class 5 Heat-Treated mechanical
Property |
Temperature |
Value |
Comment |
Charpy impact energy |
23.0 °C |
Charpy impact energy of 54 J |
- |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Medium Carbon Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 16 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Medium Carbon Steel |
Reduction of area |
23.0 °C |
Reduction of area of 43 % |
- |
Shear modulus |
23.0 °C |
Shear modulus of 75 - 80 GPa |
Typical for Carbon Steel |
Tensile strength |
23.0 °C |
Tensile strength of 900 MPa |
- |
Yield strength Rp0.02 |
23.0 °C |
Yield strength Rp0.02 of 790 - 930 MPa |
- |
Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 825 - 965 MPa |
- |