ASTM A537 Class 1 Normalized
Equivalent material: ASTM Class 2, ASTM Class 3, ASTM Class 4, ASTM Class 5, ASTM Class 6
ASTM A537 Class 1 Normalized general
Property | Value | Comment |
---|---|---|
Density | Density of 7.8 g/cm³ | Typical for Steel |
ASTM A537 Class 1 Normalized thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | Coefficient of thermal expansion of 11.94 1/K | Predicted Value |
Specific heat capacity | Specific heat capacity of 458 J/(kg·K) | Predicted Value |
Thermal conductivity | Thermal conductivity of 32.64 W/(m·K) | Predicted Value |
ASTM A537 Class 1 Normalized chemical
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | Carbon of 0.24 % | Normalized | ASTM A537 | Plate |
Chromium | Chromium of 0.25 % | Normalized | ASTM A537 | Plate |
Copper | Copper of 0.35 % | Normalized | ASTM A537 | Plate |
Manganese | Manganese of 0.7 - 1.35 % | Normalized | ASTM A537 | Plate |
Molybdenum | Molybdenum of 0.08 % | Normalized | ASTM A537 | Plate |
Nickel | Nickel of 0.25 % | Normalized | ASTM A537 | Plate |
Phosphorus | Phosphorus of 0.025 % | Normalized | ASTM A537 | Plate |
Silicon | Silicon of 0.15 - 0.5 % | Normalized | ASTM A537 | Plate |
Sulfur | Sulfur of 0.025 % | Normalized | ASTM A537 | Plate |
ASTM A537 Class 1 Normalized electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | Electrical conductivity of 7 S/m | Predicted Value |
Electrical resistivity | Electrical resistivity of 39 Ω·m | Predicted Value |
ASTM A537 Class 1 Normalized mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | Elastic modulus of 190 - 210 GPa | - | - | - | Typical for Steel |
Elongation | Elongation of 17.9 % | - | - | - | Predicted Value, A80 |
- | Elongation of 18 % | Normalized | ASTM A537 | Plate | A200 |
- | Elongation of 18.5 % | - | - | - | Predicted Value, Transverse |
- | Elongation of 19.3 % | - | - | - | Predicted Value, A80 Transverse |
- | Elongation of 22 % | Normalized | ASTM A537 | Plate | A50 |
- | Elongation of 24.7 % | - | - | - | Predicted Value |
Hardness, Brinell | Hardness, Brinell of 239 [-] | - | - | - | Predicted Value, Transverse |
Poisson's ratio | Poisson's ratio of 0.3 [-] | - | - | - | Typical for Steel |
Reduction of area | Reduction of area of 40.6 % | - | - | - | Predicted Value |
- | Reduction of area of 43.9 % | - | - | - | Predicted Value, Transverse |
Shear modulus | Shear modulus of 79.6 GPa | - | - | - | Predicted Value |
Shear strength | Shear strength of 534.1 MPa | - | - | - | Predicted Value |
Tensile strength | Tensile strength of 450 - 585 MPa | Normalized | ASTM A537 | Plate | - |
- | Tensile strength of 485 - 620 MPa | Normalized | ASTM A537 | Plate | - |
Yield strength | Yield strength of 264.2 MPa | - | - | - | Predicted Value, RP1 |
- | Yield strength of 310 MPa | Normalized | ASTM A537 | Plate | - |
- | Yield strength of 317.5 MPa | - | - | - | Predicted Value, RP1 Transverse |
- | Yield strength of 338.9 MPa | - | - | - | Predicted Value, RP05 |
- | Yield strength of 345 MPa | Normalized | ASTM A537 | Plate | - |
- | Yield strength of 345.4 MPa | - | - | - | Predicted Value, Transverse |
- | Yield strength of 378 MPa | - | - | - | Predicted Value, RP02 |
- | Yield strength of 404.9 MPa | - | - | - | Predicted Value, RP002 |
- | Yield strength of 469.4 MPa | - | - | - | Predicted Value, RP02 Transverse |
Trust our high-quality steel to forge a brighter and stronger future for your projects.
-- Our promise
Similar or equivalent steel materials
- EN 10217-3 Grade StE 420 normalized or normalized formed (+N)
- DIN 17103 Grade StE 420 cold worked, welded and normalized
- ASTM A288 Class 2 Quenched and Tempered
- ASTM A288 Class 4 Quenched and Tempered
- ASTM A288 Class 5 Quenched and Tempered
- ASTM A649 Class 2 Normalized and Tempered
- ASTM A471 Class 2 Heat-Treated
- ASTM A471 Class 4 Heat-Treated
- ASTM A471 Class 5 Heat-Treated
- ASTM A649 Class 4 Normalized, Liquid Quenched and Tempered
Get a quote