AISI 309 Cold Finished

Equivalent material: DIN 1.4828, DIN X15CrNiSi2012, DIN X15CrNiSi20-12, AFNOR Z15CNS20.12, AFNOR Z9CN24-13, BS 309S24, SAE 309, JIS SUH309, JIS SUS309TP, JIS SUS309TB, JIS SUS309TF, EN X15CrNiSi20-12, EN 1.4828, GOST 20Ch20N14S2, UNS S30900

AISI 309 Cold Finished general

Property Temperature Value
Density 23.0 °C Density of 7.8 g/cm³

AISI 309 Cold Finished thermal

Property Temperature Value
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.5E-5 1/K
Melting point - Melting point of 1400 °C
Specific heat capacity 23.0 °C Specific heat capacity of 500 J/(kg·K)
Thermal conductivity 23.0 °C Thermal conductivity of 16 W/(m·K)

AISI 309 Cold Finished chemical

Property Value
Carbon Carbon of 0 - 0.2 %
Chromium Chromium of 19 - 24 %
Iron Iron of 58 - 68.5 %
Manganese Manganese of 0 - 2 %
Nickel Nickel of 11 - 15 %
Nitrogen Nitrogen of 0 - 0.1 %
Phosphorus Phosphorus of 0 - 0.05 %
Silicon Silicon of 0 - 2.5 %
Sulfur Sulfur of 0 - 0.03 %

AISI 309 Cold Finished electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

AISI 309 Cold Finished mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 GPa -
Elongation 23.0 °C Elongation of 35 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 710 MPa -
Yield strength 23.0 °C Yield strength of 360 MPa -