AISI 304LN 1/8-Hard
Equivalent material: DIN 1.4311, DIN X2CrNiN18-10, AFNOR Z3CN18-10, BS 304S62, UNI X2CrNiN1810, SS 2371, SAE 304LN, JIS SUS304LN, JIS SUSF304LN, EN X2CrNiN18-10, EN 1.4311, GB 00Cr18Ni10N, UNS S30453, ASTM TP304LN, ASTM 304LN, ASTM S30453, ASTM F304LN, ASTM Grade 8LN, ASTM S30454, UNS S30454
AISI 304LN 1/8-Hard general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
AISI 304LN 1/8-Hard thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
- |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 500 J/(kg·K) |
- |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 15 W/(m·K) |
- |
AISI 304LN 1/8-Hard chemical
Property |
Value |
Carbon |
Carbon of 0 - 0.03 % |
Chromium |
Chromium of 17.5 - 20 % |
Iron |
Iron of 65 - 73.9 % |
Manganese |
Manganese of 0 - 2 % |
Nickel |
Nickel of 8 - 12 % |
Nitrogen |
Nitrogen of 0.1 - 0.22 % |
Phosphorus |
Phosphorus of 0 - 0.05 % |
Silicon |
Silicon of 0 - 1 % |
Sulfur |
Sulfur of 0 - 0.03 % |
AISI 304LN 1/8-Hard electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
AISI 304LN 1/8-Hard mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 GPa |
- |
Elongation |
23.0 °C |
Elongation of 38 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 790 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 440 MPa |
- |