AISI 301LN 1/8-Hard
Equivalent material: DIN 1.4424, DIN X2CrNiMoSi19-5, AFNOR Z2CND18-05-03, SS 2376, SAE 301LN, EN X2CrNiMoSi18-5-3, EN 1.4424, ASTM 301LN, UNS S31500
AISI 301LN 1/8-Hard general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
AISI 301LN 1/8-Hard thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.2E-5 1/K |
- |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 500 J/(kg·K) |
- |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 15 W/(m·K) |
- |
AISI 301LN 1/8-Hard chemical
Property |
Value |
Carbon |
Carbon of 0 - 0.03 % |
Chromium |
Chromium of 16 - 18.5 % |
Iron |
Iron of 70.2 - 77.9 % |
Manganese |
Manganese of 0 - 2 % |
Nickel |
Nickel of 6 - 8 % |
Nitrogen |
Nitrogen of 0.07 - 0.2 % |
Phosphorus |
Phosphorus of 0 - 0.05 % |
Silicon |
Silicon of 0 - 1 % |
Sulfur |
Sulfur of 0 - 0.03 % |
AISI 301LN 1/8-Hard electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
AISI 301LN 1/8-Hard mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 GPa |
- |
Elongation |
23.0 °C |
Elongation of 40 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 870 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 480 MPa |
- |