SAE J405 Grade 304L
Equivalent material: DIN 1.4306, DIN X2CrNi19-11, DIN 19Cr11Ni, AFNOR Z3CN18-10, BS 304S11, SS 2352, AISI 304L, JIS SUS304L, JIS SCS19, JIS SCS19A, JIS SUS304LTB, JIS SUS304LTP, JIS SUS304LTPY, JIS SUS304LTBS, JIS SUSF304L, EN X2CrNi19-11, EN 1.4306, ISO A3, GB 00Cr19Ni10, ASTM Grade CPF3, UNS S30403, DIN 1.4307, DIN G-X2CrNiN18-9, AFNOR Z3CN19-09, EN X2CrNi18-9, EN 1.4307, GOST 03Ch18N11, ASTM TP304L, IS X02Cr18Ni11, DIN 1.4309, BS 304C12, JIS SCS13, EN GX2CrNi19-11, EN 1.4309, ASTM CF3, UNS J92500, ASTM 304L, ASTM S30403, ASTM F304L, ASTM MT304L
SAE J405 Grade 304L general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
SAE J405 Grade 304L thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
SAE J405 Grade 304L chemical
Property |
Value |
Carbon |
Carbon of 0.03 % |
Chromium |
Chromium of 18 - 20 % |
Manganese |
Manganese of 2 % |
Nickel |
Nickel of 8 - 12 % |
Nitrogen |
Nitrogen of 0.1 % |
Phosphorus |
Phosphorus of 0.05 % |
Silicon |
Silicon of 0.75 % |
Sulfur |
Sulfur of 0.03 % |
SAE J405 Grade 304L electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
SAE J405 Grade 304L mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |