JIS G5122 Grade SCH12

Equivalent material: DIN G-X25CrNiSi18-9, DIN G-X40CrNiSi22-9, BS 302C35, UNI GX16CrNi2010, UNE AM-X7CrNi2010, UNE AM-X30CrNi2010, AMS 5358, ASTM HF, ASTM CF20, GB/T ZG30Cr20Ni10, DIN 1.4826, DIN GX40CrNiSi22-9, JIS SCH22, EN GX40CrNiSi22-9, EN 1.4826, ISO GX40CrNiSi22-9

JIS G5122 Grade SCH12 general

Property Temperature Value Comment
Density 23.0 °C Density of 7.9 - 8.2 g/cm³ Typical for Austenitic Stainless Steel

JIS G5122 Grade SCH12 thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K Typical for Austenitic Stainless Steel
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 J/(kg·K) Typical for Austenitic Stainless Steel
Thermal conductivity 23.0 °C Thermal conductivity of 11 - 21 W/(m·K) Typical for Austenitic Stainless Steel

JIS G5122 Grade SCH12 electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

JIS G5122 Grade SCH12 mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 195 GPa Typical for Austenitic Stainless Steel
Elongation A5 23.0 °C Elongation A5 of 23 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 490 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 235 MPa -

Experience the power of our steel, meticulously crafted to withstand the toughest challenges and meet the highest industry standards.

-- Our promise

Similar or equivalent steel materials