JIS G4801 Grade SUP13
Equivalent material: BS BW4, ASTM 4161, AISI 4161, SAE 4161, DIN 1.7241, DIN 60CrMo3-3, AFNOR 60CrMo3-3, BS 60CrMo3-3, BS 705A60, AISI 4161H, SAE 4161H, EN 60CrMo3-3, EN 1.7241, ASTM 4161H, UNS H41610, UNS G41610
JIS G4801 Grade SUP13 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Molybdenum Steel |
JIS G4801 Grade SUP13 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K |
Typical for Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 502 J/(kg·K) |
Typical for Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 36 - 43 W/(m·K) |
Typical for Chromium Molybdenum Steel |
JIS G4801 Grade SUP13 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Molybdenum Steel |
Elongation A5 |
23.0 °C |
Elongation A5 of 10 % |
- |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 363 - 429 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Molybdenum Steel |
Reduction of area |
23.0 °C |
Reduction of area of 30 % |
- |
Tensile strength |
23.0 °C |
Tensile strength of 1226 MPa |
- |
Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 1079 MPa |
- |