JIS G4307 Grade SUS347 cold-rolled and solution annealed
Equivalent material: GB 1Cr19Ni11Nb, GB/T 0Cr18Ni11Nb, GB/T 0Cr18Ni11Nb-Q, GB/T 0Cr18Ni11Nb-R, GB 0Cr18Ni11Nb, GB 1Cr19Ni11Nb, GB 1Cr18ni11Nb, GOST 08Х18Н12Б, GOST 08H18N12B, DIN X6CrNiNb1810, EN X6CrNiNb18-10, NF Z6CNNb18-10, BS 347S17, BS 821Nb, BS 347S31, BS 347S51, BS 347S59, IS 04Cr18Ni10Nb40, IS O4Cr18Ni10Nb40, UNI X6CrNiNb1811, UNI X6CrNiNb1811KT, UNI X8CrNiNb1811, UNI X6CrNiNb1811KG, UNI X6CrNiNb1811KW, ÖNORM X6CrNiNb1810S, ÖNORM X6CrNiNb1810KKW, UNE X6CrNiNb1811, UNE X7CrNiNb1811, UNE X6CrNiNb1810, SIS 2338-02, SIS 2338-22, SIS 2338-23, SIS 2338-24, SIS 2338-25, SIS 2338-26, SIS 2338-27, SIS 2338-29, SIS 2338, AMS 5512, AMS 5556, AMS 5571, AMS 5575, AMS 5654, AMS 5674, AMS 7229, AMS 7490, ASME 347, ASTM TP347, ASTM 347, ASTM B8C, ASTM B8CA, ASTM CR347, ASTM WP347, ASTM F347, ASTM 8C, ASTM FP347, ASTM MT347, ASTM 8CA, MIL 347, MIL CTP-347, JIS SUS347TB, JIS SUS347TKA, JIS SUS347TP, JIS SUSF347, AISI 347, SAE 347, BS 2S.130, BS 2S.143, BS 2S.144, BS 2S.145, BS S.525, BS S.527, UNI G-X6CrNiNb1811, ASME 348, ASTM TP348, ASTM 348, ASTM CR348, ASTM WP348, ASTM F348, MIL 348, AISI 348, SAE 348, ASTM S34700, ASTM Grade F347, ASTM Grade B8C, ASTM Grade B8CA, UNS S34700, ASTM Grade 8C, DIN 1.4550, DIN X6CrNiNb18-10, DIN X10CrNiNb, AFNOR Z6CNNb18-10, SS 2338, UNE F.3552, UNE F.3524, AISI 347H, SAE 347H, JIS SUS347TPY, JIS SUS347TF, JIS SUS347FB, EN 1.4550, ASTM S34709, ASTM Grade F347H, UNS S34709
JIS G4307 Grade SUS347 cold-rolled and solution annealed general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
JIS G4307 Grade SUS347 cold-rolled and solution annealed thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
JIS G4307 Grade SUS347 cold-rolled and solution annealed electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
JIS G4307 Grade SUS347 cold-rolled and solution annealed mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Elongation |
23.0 °C |
Elongation of 40 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 520 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 206 MPa |
- |