JIS G4307 Grade SUS317L

Equivalent material: GB/T 00Cr19Ni13Mo3, GB/T 0Cr18Ni16Mo5, GB 00Cr19Ni13Mo3, GB 0Cr18Ni16Mo5, GB 00Cr17Ni14Mo3, AS 317L, DIN X2CrNiMo18164, EN X2CrNiMo18-15-4, NF Z2CND19-15, NF Z2CND19-14, NF Z3CND19-15-04, NF Z2CND19-15-04, BS 317S12, UNI X2CrNiMo1816, UNI X2CrNiMo1815, ÖNORM X2CrNiMo18164KW, UNE X2CrNiMo18164, SIS 2367, ASME 317L, ASTM TP317L, ASTM CR317L, ASTM WP317L, ASTM 317L, ASTM 19Cr 13Ni 3.5Mo, ASTM F317L, JIS SUS317LTP, AISI 317L, SAE 317L, UNS S31703, DIN 1.4438, DIN X2CrNiMo18-16-4, DIN X2CrNiMo18-15-4, AFNOR Z3CND19-15-04, SS 2367, UNE F.3539, AISI TP 317L, SAE TP 317L, JIS SUS317LTPY, JIS SUS317LTB, JIS SUS317LFB, JIS SUSF317L, EN 1.4438, UNS S31700

JIS G4307 Grade SUS317L general

Property Temperature Value Comment
Density 23.0 °C Density of 7.9 - 8.2 g/cm³ Typical for Austenitic Stainless Steel

JIS G4307 Grade SUS317L thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K Typical for Austenitic Stainless Steel
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 J/(kg·K) Typical for Austenitic Stainless Steel
Thermal conductivity 23.0 °C Thermal conductivity of 11 - 21 W/(m·K) Typical for Austenitic Stainless Steel

JIS G4307 Grade SUS317L chemical

Property Value
Carbon Carbon of 0.03 %
Chromium Chromium of 18 - 20 %
Iron Iron of 57.89 - 68 %
Manganese Manganese of 2 %
Molybdenum Molybdenum of 3 - 4 %
Nickel Nickel of 11 - 15 %
Phosphorus Phosphorus of 0.05 %
Silicon Silicon of 1 %
Sulfur Sulfur of 0.03 %

JIS G4307 Grade SUS317L electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

JIS G4307 Grade SUS317L mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 195 GPa Typical for Austenitic Stainless Steel
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel