JIS G3506 Grade SWRH57A
Equivalent material: DIN 1.0609, DIN D 58-2, DIN C58D, AFNOR C58D, BS C58D, AISI 1060, SAE 1060, JIS SWRH57, JIS CS55, EN C58D, EN 1.0609, ISO C58D, GB/T C58D, GB/T U53582, ASTM 1060, UNS G10600
JIS G3506 Grade SWRH57A general
| Property |
Temperature |
Value |
Comment |
| Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Medium Carbon Steel |
JIS G3506 Grade SWRH57A thermal
| Property |
Temperature |
Value |
Comment |
| Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.32E-5 1/K |
Typical for Medium Carbon Steel |
| Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
| Melting point |
- |
Melting point of 1380 - 1514 °C |
Typical for Medium Carbon Steel |
| Specific heat capacity |
23.0 °C |
Specific heat capacity of 470 - 520 J/(kg·K) |
Typical for Medium Carbon Steel |
| Thermal conductivity |
23.0 °C |
Thermal conductivity of 21 - 52 W/(m·K) |
Typical for Medium Carbon Steel |
JIS G3506 Grade SWRH57A chemical
| Property |
Value |
| Carbon |
Carbon of 0.54 - 0.61 % |
| Iron |
Iron of 98.38 - 99.01 % |
| Manganese |
Manganese of 0.3 - 0.6 % |
| Phosphorus |
Phosphorus of 0.03 % |
| Silicon |
Silicon of 0.15 - 0.35 % |
| Sulfur |
Sulfur of 0.03 % |
JIS G3506 Grade SWRH57A electrical
| Property |
Temperature |
Value |
Comment |
| Electrical resistivity |
23.0 °C |
Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m |
Typical for Carbon Steel |
JIS G3506 Grade SWRH57A mechanical
| Property |
Temperature |
Value |
Comment |
| Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Medium Carbon Steel |
| Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Medium Carbon Steel |
| Shear modulus |
23.0 °C |
Shear modulus of 75 - 80 GPa |
Typical for Carbon Steel |