JIS G3468 Grade SUS347TPY

Equivalent material: DIN 1.4550, DIN X6CrNiNb18-10, DIN X10CrNiNb, AFNOR Z6CNNb18-10, BS 347S17, UNI X6CrNiNb1811, SS 2338, UNE F.3552, UNE F.3524, AISI 347H, SAE 347H, JIS SUS347, JIS SUS347TP, JIS SUS347TF, JIS SUS347TKA, JIS SUS347FB, JIS SUS347TB, EN X6CrNiNb18-10, EN 1.4550, ASTM S34709, ASTM Grade F347H, UNS S34709

JIS G3468 Grade SUS347TPY general

Property Temperature Value Comment
Density 23.0 °C Density of 7.9 - 8.2 g/cm³ Typical for Austenitic Stainless Steel

JIS G3468 Grade SUS347TPY thermal

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 195 GPa Typical for Austenitic Stainless Steel
Elongation A5 23.0 °C Elongation A5 of 18 - 35 % -
Elongation A5, transverse 23.0 °C Elongation A5, transverse of 25 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 520 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 205 MPa -

JIS G3468 Grade SUS347TPY magnetic

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

JIS G3468 Grade SUS347TPY electrical

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K Typical for Austenitic Stainless Steel
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 J/(kg·K) Typical for Austenitic Stainless Steel
Thermal conductivity 23.0 °C Thermal conductivity of 11 - 21 W/(m·K) Typical for Austenitic Stainless Steel

JIS G3468 Grade SUS347TPY mechanical

Property Value
Wall thickness Wall thickness of 2 - 8 mm

Trust our expertise to deliver precision-engineered steel solutions that meet the highest industry standards.