JIS G3467 Grade SUS321HTF
Equivalent material: DIN 1.4878, DIN X12CrNiTi18-9, DIN X8CrNiTi18-10, AFNOR X8CrNiTi18-10, JIS SUS321, JIS SUS321HTB, JIS SUS321HTP, JIS SUS321TKA, EN X8CrNiTi18-10, EN 1.4878, GOST 08X18H10T, GOST 12X18H10T, ASTM Type 321
JIS G3467 Grade SUS321HTF general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
JIS G3467 Grade SUS321HTF thermal
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Elongation A5 |
23.0 °C |
Elongation A5 of 16 - 35 % |
- |
Elongation A5, transverse |
23.0 °C |
Elongation A5, transverse of 22 - 25 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 520 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 205 MPa |
- |
JIS G3467 Grade SUS321HTF magnetic
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
JIS G3467 Grade SUS321HTF electrical
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
JIS G3467 Grade SUS321HTF mechanical
Property |
Value |
Wall thickness |
Wall thickness of 1 - 8 mm |