EN 10277-2 Grade St 37-3 cold drawn or turned and normalized
EN 10277-2 Grade St 37-3 cold drawn or turned and normalized introduction
St 37-3 is a fine grained structural steel and used stress dependent for welded constructions up to a temperature of -25 °C.
Equivalent material: NBN AE235-D, AFNOR E-24-4, BS 40D, GOST S235, ISO Fe360-C, ISO Fe360-D, UNI F360D, ÖNORM St360D, UNE AE235D, ASTM D, DIN S235J2G3, DIN 1.0116, DIN S235J2, AFNOR TU E 235 4, AFNOR S235J2G3, AFNOR E24-2, BS HFS 4, BS S235J2G3, AISI 1513, SAE 1513, JIS SS330, EN S235J2G3, EN 1.0116, GOST St3ps, GOST St3sp, GOST 16D, GB/T Q235A, GB/T U12352, ASTM Grade Ib, UNS K02701, UNS K02601, UNS K01702
EN 10277-2 Grade St 37-3 cold drawn or turned and normalized general
Property |
Temperature |
Value |
Density |
20.0 °C |
Density of 7.85 g/cm³ |
EN 10277-2 Grade St 37-3 cold drawn or turned and normalized thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
-100.0 °C |
Coefficient of thermal expansion of 1.08E-5 1/K |
- |
- |
20.0 °C |
Coefficient of thermal expansion of 1.19E-5 1/K |
- |
- |
100.0 °C |
Coefficient of thermal expansion of 1.25E-5 1/K |
- |
- |
200.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
- |
- |
300.0 °C |
Coefficient of thermal expansion of 1.36E-5 1/K |
- |
- |
400.0 °C |
Coefficient of thermal expansion of 1.41E-5 1/K |
- |
- |
500.0 °C |
Coefficient of thermal expansion of 1.45E-5 1/K |
- |
- |
600.0 °C |
Coefficient of thermal expansion of 1.49E-5 1/K |
- |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Max service temperature, long |
- |
Max service temperature, long of -20 - 0 °C |
- |
Melting point |
- |
Melting point of 1480 - 1526 °C |
Typical for Low Carbon Steel |
Specific heat capacity |
-100.0 °C |
Specific heat capacity of 423 J/(kg·K) |
- |
- |
20.0 °C |
Specific heat capacity of 461 J/(kg·K) |
- |
- |
100.0 °C |
Specific heat capacity of 479 J/(kg·K) |
- |
- |
200.0 °C |
Specific heat capacity of 499 J/(kg·K) |
- |
- |
300.0 °C |
Specific heat capacity of 517 J/(kg·K) |
- |
- |
400.0 °C |
Specific heat capacity of 536 J/(kg·K) |
- |
- |
500.0 °C |
Specific heat capacity of 558 J/(kg·K) |
- |
- |
600.0 °C |
Specific heat capacity of 587 J/(kg·K) |
- |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 56.9 W/(m·K) |
- |
- |
100.0 °C |
Thermal conductivity of 56.4 W/(m·K) |
- |
- |
200.0 °C |
Thermal conductivity of 53.5 W/(m·K) |
- |
- |
300.0 °C |
Thermal conductivity of 49.4 W/(m·K) |
- |
- |
400.0 °C |
Thermal conductivity of 45.2 W/(m·K) |
- |
- |
500.0 °C |
Thermal conductivity of 41.3 W/(m·K) |
- |
- |
600.0 °C |
Thermal conductivity of 37.6 W/(m·K) |
- |
Thermal diffusivity |
20.0 °C |
Thermal diffusivity of 15.7 mm²/s |
- |
- |
100.0 °C |
Thermal diffusivity of 14.5 mm²/s |
- |
- |
200.0 °C |
Thermal diffusivity of 12.9 mm²/s |
- |
- |
300.0 °C |
Thermal diffusivity of 11.2 mm²/s |
- |
- |
400.0 °C |
Thermal diffusivity of 9.6 mm²/s |
- |
- |
500.0 °C |
Thermal diffusivity of 7.9 mm²/s |
- |
- |
600.0 °C |
Thermal diffusivity of 6.3 mm²/s |
- |
EN 10277-2 Grade St 37-3 cold drawn or turned and normalized chemical
Property |
Value |
Aluminium |
Aluminium of 0.02 % |
Carbon |
Carbon of 0.17 % |
Phosphorus |
Phosphorus of 0.04 % |
Sulfur |
Sulfur of 0.04 % |
EN 10277-2 Grade St 37-3 cold drawn or turned and normalized magnetic
Property |
Value |
Comment |
Curie temperature |
Curie temperature of 770 °C |
Typical for Low Carbon Steel |
EN 10277-2 Grade St 37-3 cold drawn or turned and normalized electrical
Property |
Temperature |
Value |
Electrical resistivity |
20.0 °C |
Electrical resistivity of 1.83E-7 Ω·m |
- |
100.0 °C |
Electrical resistivity of 2.27E-7 Ω·m |
- |
200.0 °C |
Electrical resistivity of 2.95E-7 Ω·m |
- |
300.0 °C |
Electrical resistivity of 3.8E-7 Ω·m |
- |
400.0 °C |
Electrical resistivity of 4.81E-7 Ω·m |
- |
500.0 °C |
Electrical resistivity of 5.99E-7 Ω·m |
- |
600.0 °C |
Electrical resistivity of 7.38E-7 Ω·m |
EN 10277-2 Grade St 37-3 cold drawn or turned and normalized mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
-100.0 °C |
Elastic modulus of 217 GPa |
- |
- |
20.0 °C |
Elastic modulus of 212 GPa |
- |
- |
100.0 °C |
Elastic modulus of 207 GPa |
- |
- |
200.0 °C |
Elastic modulus of 199 GPa |
- |
- |
300.0 °C |
Elastic modulus of 192 GPa |
- |
- |
400.0 °C |
Elastic modulus of 184 GPa |
- |
- |
500.0 °C |
Elastic modulus of 175 GPa |
- |
- |
600.0 °C |
Elastic modulus of 164 GPa |
- |
Elongation |
20.0 °C |
Elongation of 24 - 26 % |
- |
Poisson's ratio |
20.0 °C |
Poisson's ratio of 0.28 [-] |
- |
Shear modulus |
23.0 °C |
Shear modulus of 82 GPa |
Typical for Low Carbon Steel |
Tensile strength |
20.0 °C |
Tensile strength of 340 - 470 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 215 - 235 MPa |
- |