EN 10149-2 Grade S500MC thermomechanically rolled
EN 10149-2 Grade S500MC thermomechanically rolled introduction
The thermomechanical rolled steel is used for cold formed components like vehicle frames, axles and special sections.
Equivalent material: AFNOR E490D, IS HSF490, IS FeE500, ASTM A1011 HSLAS-F Grade 70, ASTM A1011 Grade 070, DIN QStE500TM, DIN HR500LA, ASTM HSLAS-F70, DIN 1.0984, EN QStE 500 TM, EN 1.0984, DIN QStE 500 TM, DIN S500MC, AFNOR S500MC, AFNOR S490MC, UNE AE490HC, BS S500MC, ISO HSF490, ISO FeE500, ISO FeE490, ASTM HSLAS Grade 480 Class 1, ASTM HSLAS Grade 480 Class 2, ASTM HSLAS-F Grade 480
EN 10149-2 Grade S500MC thermomechanically rolled general
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20 °C | Density of 7.84 g/cm³ | thermomechanically rolled | EN 10149-2 | Flat |
EN 10149-2 Grade S500MC thermomechanically rolled thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | -100 °C | Coefficient of thermal expansion of 1.08e-05 1/K | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 20 °C | Coefficient of thermal expansion of 1.19e-05 1/K | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 100 °C | Coefficient of thermal expansion of 1.25e-05 1/K | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 200 °C | Coefficient of thermal expansion of 1.3e-05 1/K | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 300 °C | Coefficient of thermal expansion of 1.36e-05 1/K | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 400 °C | Coefficient of thermal expansion of 1.41e-05 1/K | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 500 °C | Coefficient of thermal expansion of 1.45e-05 1/K | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 600 °C | Coefficient of thermal expansion of 1.49e-05 1/K | thermomechanically rolled | EN 10149-2 | Flat | - |
Max service temperature | - | Max service temperature of -20 °C | thermomechanically rolled | EN 10149-2 | Flat | Long |
- | - | Max service temperature of 500 °C | - | - | - | Typical for Carbon Steel |
Melting point | - | Melting point of 1480 - 1526 °C | - | - | - | Typical for Low Carbon Steel |
Specific heat capacity | -100 °C | Specific heat capacity of 423 J/(kg·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 20 °C | Specific heat capacity of 461 J/(kg·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 100 °C | Specific heat capacity of 479 J/(kg·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 200 °C | Specific heat capacity of 499 J/(kg·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 300 °C | Specific heat capacity of 517 J/(kg·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 400 °C | Specific heat capacity of 536 J/(kg·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 500 °C | Specific heat capacity of 558 J/(kg·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 600 °C | Specific heat capacity of 587 J/(kg·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
Thermal conductivity | -100 °C | Thermal conductivity of 46.5 W/(m·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 20 °C | Thermal conductivity of 49.4 W/(m·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 100 °C | Thermal conductivity of 49.4 W/(m·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 200 °C | Thermal conductivity of 47.8 W/(m·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 300 °C | Thermal conductivity of 45.1 W/(m·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 400 °C | Thermal conductivity of 41.8 W/(m·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 500 °C | Thermal conductivity of 38.6 W/(m·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 600 °C | Thermal conductivity of 35.3 W/(m·K) | thermomechanically rolled | EN 10149-2 | Flat | - |
Thermal diffusivity | -100 °C | Thermal diffusivity of 15.9 mm²/s | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 20 °C | Thermal diffusivity of 13.7 mm²/s | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 100 °C | Thermal diffusivity of 12.7 mm²/s | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 200 °C | Thermal diffusivity of 11.5 mm²/s | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 300 °C | Thermal diffusivity of 10.2 mm²/s | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 400 °C | Thermal diffusivity of 8.9 mm²/s | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 500 °C | Thermal diffusivity of 7.4 mm²/s | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 600 °C | Thermal diffusivity of 5.8 mm²/s | thermomechanically rolled | EN 10149-2 | Flat | - |
EN 10149-2 Grade S500MC thermomechanically rolled chemical
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | Aluminium of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Carbon | Carbon of 0.12 % | thermomechanically rolled | EN 10149-2 | Flat |
Manganese | Manganese of 1.7 % | thermomechanically rolled | EN 10149-2 | Flat |
Niobium | Niobium of 0.09 % | thermomechanically rolled | EN 10149-2 | Flat |
Phosphorus | Phosphorus of 0.025 % | thermomechanically rolled | EN 10149-2 | Flat |
Silicon | Silicon of 0.5 % | thermomechanically rolled | EN 10149-2 | Flat |
Sulfur | Sulfur of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Titanium | Titanium of 0.15 % | thermomechanically rolled | EN 10149-2 | Flat |
Vanadium | Vanadium of 0.2 % | thermomechanically rolled | EN 10149-2 | Flat |
EN 10149-2 Grade S500MC thermomechanically rolled magnetic
Property | Value | Comment |
---|---|---|
Curie temperature | Curie temperature of 770 °C | Typical for Low Carbon Steel |
EN 10149-2 Grade S500MC thermomechanically rolled electrical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Electrical conductivity | - | Electrical conductivity of 7 S/m | - | - | - | Predicted Value |
Electrical resistivity | -100 °C | Electrical resistivity of 1.47e-07 Ω·m | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 20 °C | Electrical resistivity of 2.11e-07 Ω·m | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 100 °C | Electrical resistivity of 2.59e-07 Ω·m | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 200 °C | Electrical resistivity of 3.3e-07 Ω·m | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 300 °C | Electrical resistivity of 4.16e-07 Ω·m | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 400 °C | Electrical resistivity of 5.2e-07 Ω·m | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 500 °C | Electrical resistivity of 6.41e-07 Ω·m | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 600 °C | Electrical resistivity of 7.85e-07 Ω·m | thermomechanically rolled | EN 10149-2 | Flat | - |
EN 10149-2 Grade S500MC thermomechanically rolled mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | -100 °C | Elastic modulus of 217 GPa | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 20 °C | Elastic modulus of 212 GPa | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 100 °C | Elastic modulus of 207 GPa | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 200 °C | Elastic modulus of 199 GPa | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 300 °C | Elastic modulus of 192 GPa | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 400 °C | Elastic modulus of 184 GPa | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 500 °C | Elastic modulus of 175 GPa | thermomechanically rolled | EN 10149-2 | Flat | - |
- | 600 °C | Elastic modulus of 164 GPa | thermomechanically rolled | EN 10149-2 | Flat | - |
Elongation | - | Elongation of 13.9 % | - | - | - | Predicted Value, A200 |
- | - | Elongation of 14.1 % | - | - | - | Predicted Value, Transverse |
- | - | Elongation of 15.8 % | - | - | - | Predicted Value, A80 Transverse |
- | - | Elongation of 17.8 % | - | - | - | Predicted Value, A50 |
- | - | Elongation of 21.1 % | - | - | - | Predicted Value, A5 |
- | 20 °C | Elongation of 12 % | thermomechanically rolled | EN 10149-2 | Flat | A80 |
- | 20 °C | Elongation of 14 % | thermomechanically rolled | EN 10149-2 | Flat | - |
Hardness, Brinell | - | Hardness, Brinell of 245 [-] | - | - | - | Predicted Value, Transverse |
Poisson's ratio | - | Poisson's ratio of 0.29 [-] | - | - | - | Typical for Low Carbon Steel |
Reduction of area | - | Reduction of area of 39.1 % | - | - | - | Predicted Value |
- | - | Reduction of area of 44.2 % | - | - | - | Predicted Value, Transverse |
Shear modulus | - | Shear modulus of 82 GPa | - | - | - | Typical for Low Carbon Steel |
Shear strength | - | Shear strength of 501.6 MPa | - | - | - | Predicted Value |
Tensile strength | 20 °C | Tensile strength of 550 - 700 MPa | thermomechanically rolled | EN 10149-2 | Flat | - |
Yield strength | - | Yield strength of 265.3 MPa | - | - | - | Predicted Value, RP1 |
- | - | Yield strength of 298.9 MPa | - | - | - | Predicted Value, RP1 Transverse |
- | - | Yield strength of 435.8 MPa | - | - | - | Predicted Value, Transverse |
- | - | Yield strength of 466.5 MPa | - | - | - | Predicted Value, RP02 |
- | - | Yield strength of 484.2 MPa | - | - | - | Predicted Value, RP02 Transverse |
- | - | Yield strength of 486.3 MPa | - | - | - | Predicted Value, RP05 |
- | - | Yield strength of 519.8 MPa | - | - | - | Predicted Value, RP002 |
- | 20 °C | Yield strength of 500 MPa | thermomechanically rolled | EN 10149-2 | Flat | - |
Our steel products inspire endless possibilities while ensuring engineering excellence.
-- Our promise
Similar or equivalent steel materials
- EN 10149-2 Grade S460MC thermomechanically rolled
- ASTM A1018 HSLAS Grade 450 Class 1
- ASTM A1018 HSLAS Grade 480 Class 2
- ASTM A1018 HSLAS Grade 450 Class 2
- ASTM A1018 HSLAS Grade 480 Class 1
- ASTM A1018 HSLAS-F Grade 480
- ASTM A1011 HSLAS Grade 480 Class 2
- ASTM A1011 HSLAS-F Grade 480
- ASTM A1008 HSLAS-F Grade 480
- ASTM A1008 HSLAS Grade 450 Class 1
Get a quote