DIN 2391-2 Grade St 45 bright drawn and stress relieved
DIN 2391-2 Grade St 45 bright drawn and stress relieved introduction
Seamless precision steel tube made from St 45 is mainly used as construction element with special requirements in dimension accuracy, small wall thicknesses and good surface condition. The tubes are made in different grades (A and C). Grade C is valid for conduits.
Grade A: for mechanical load without special grade requirement, without inspection certificate
Grade C: for special requirements (testing after arrangement, e.g. bending, flanging, bulging a.o.)
The weldability is given.
Equivalent material: BS CFS4, GOST 20, UNI Fe45-1, SS 1412, ASTM 1020, DIN DINEN10305-1, DIN 1.0408, DIN S255GT, DIN E255, BS E255, JIS STAM440G, JIS STAM440H, JIS STKM13B, JIS 13B, EN E255, EN 1.0408, ASTM Grade 1020
DIN 2391-2 Grade St 45 bright drawn and stress relieved general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Low Carbon Steel |
DIN 2391-2 Grade St 45 bright drawn and stress relieved thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K |
Typical for Low Carbon Steel |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Max service temperature, long |
- |
Max service temperature, long of 0 - 300 °C |
- |
Melting point |
- |
Melting point of 1480 - 1526 °C |
Typical for Low Carbon Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 465 J/(kg·K) |
Typical for Low Carbon Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 25 - 93 W/(m·K) |
Typical for Low Carbon Steel |
DIN 2391-2 Grade St 45 bright drawn and stress relieved chemical
Property |
Value |
Carbon |
Carbon of 0.21 % |
Manganese |
Manganese of 0.4 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.35 % |
Sulfur |
Sulfur of 0.025 % |
DIN 2391-2 Grade St 45 bright drawn and stress relieved magnetic
Property |
Value |
Comment |
Curie temperature |
Curie temperature of 770 °C |
Typical for Low Carbon Steel |
DIN 2391-2 Grade St 45 bright drawn and stress relieved electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m |
Typical for Carbon Steel |
DIN 2391-2 Grade St 45 bright drawn and stress relieved mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Low Carbon Steel |
Elongation |
20.0 °C |
Elongation of 12 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Low Carbon Steel |
Shear modulus |
23.0 °C |
Shear modulus of 82 GPa |
Typical for Low Carbon Steel |
Tensile strength |
20.0 °C |
Tensile strength of 520 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 375 MPa |
- |
Our skilled craftsmen work tirelessly to produce steel products of the highest quality and precision.
-- Our promise
Similar or equivalent steel materials