DIN 17140-1 Grade D63-2
DIN 17140-1 Grade D63-2 introduction
Non-alloy steel wire rod for cold drawing for general purpose rod
Equivalent material: GB C62D, GB U53622, IS nan, JIS SWRH62A, JIS SWRH62B, DIN 1.0611, DIN C62D, AFNOR C62D, BS C62D, AISI 1065, SAE 1065, JIS SWRH62, JIS CS65, EN C62D, EN 1.0611, ISO C62D, GB/T C62D, GB/T U53622, GB/T U59622, UNS G10650
DIN 17140-1 Grade D63-2 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for High Carbon Steel |
DIN 17140-1 Grade D63-2 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.32E-5 1/K |
Typical for High Carbon Steel |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Melting point |
- |
Melting point of 1289 - 1478 °C |
Typical for High Carbon Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 486 J/(kg·K) |
Typical for High Carbon Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 36 W/(m·K) |
Typical for High Carbon Steel |
DIN 17140-1 Grade D63-2 chemical
Property |
Value |
Carbon |
Carbon of 0.6 - 0.65 % |
Manganese |
Manganese of 0.3 - 0.7 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.1 - 0.3 % |
Sulfur |
Sulfur of 0.04 % |
DIN 17140-1 Grade D63-2 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m |
Typical for Carbon Steel |
DIN 17140-1 Grade D63-2 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for High Carbon Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for High Carbon Steel |
Shear modulus |
23.0 °C |
Shear modulus of 81 GPa |
Typical for High Carbon Steel |