ASTM A693 Grade XM-25 Solution-Treated
Equivalent material: DIN 1.4594, AFNOR Z7CNU15-05, EN X5CrNiMoCuNb14-5, EN 1.4594, ASTM 14-5PH, UNS S45000, UNS S15500
ASTM A693 Grade XM-25 Solution-Treated general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
Typical for Steel |
ASTM A693 Grade XM-25 Solution-Treated chemical
Property |
Value |
Carbon |
Carbon of 0.05 % |
Chromium |
Chromium of 14 - 16 % |
Copper |
Copper of 1.25 - 1.75 % |
Manganese |
Manganese of 1 % |
Molybdenum |
Molybdenum of 0.5 - 1 % |
Nickel |
Nickel of 5 - 7 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 1 % |
Sulfur |
Sulfur of 0.03 % |
ASTM A693 Grade XM-25 Solution-Treated mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 190 - 210 GPa |
Typical for Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 4 % |
- |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 255 - 311 [-] |
- |
Hardness, Rockwell C |
23.0 °C |
Hardness, Rockwell C of 25 - 33 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Steel |
Tensile strength |
23.0 °C |
Tensile strength of 895 - 1205 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 620 - 1035 MPa |
- |