Property Temperature Value Comment
Density 23.0 °C Density of 7.9 - 8.2 g/cm³ Typical for Austenitic Stainless Steel

ASTM A479 Grade 347 Annealed thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K Typical for Austenitic Stainless Steel
Melting point - Melting point of 1230 - 1480 °C Typical for Austenitic Stainless Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 J/(kg·K) Typical for Austenitic Stainless Steel
Thermal conductivity 23.0 °C Thermal conductivity of 11 - 21 W/(m·K) Typical for Austenitic Stainless Steel

ASTM A479 Grade 347 Annealed chemical

Property Value
Carbon Carbon of 0.08 %
Chromium Chromium of 17 - 19 %
Manganese Manganese of 2 %
Nickel Nickel of 9 - 12 %
Phosphorus Phosphorus of 0.05 %
Silicon Silicon of 1 %
Sulfur Sulfur of 0.03 %

ASTM A479 Grade 347 Annealed electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 8.5E-7 Ω·m Typical for Austenitic Stainless Steel

ASTM A479 Grade 347 Annealed mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 195 GPa Typical for Austenitic Stainless Steel
Elongation A50 23.0 °C Elongation A50 of 30 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Austenitic Stainless Steel
Reduction of area 23.0 °C Reduction of area of 40 % -
Shear modulus 23.0 °C Shear modulus of 77 GPa Typical for Austenitic Stainless Steel
Tensile strength 23.0 °C Tensile strength of 515 MPa -
Yield strength Rp0.2 23.0 °C Yield strength Rp0.2 of 205 MPa -

Our customized steel solutions ensure the perfect fit for your specific project requirements.