ASTM A471 Class 13 Heat-Treated

Equivalent material: ASTM Class 11, ASTM Class 12

ASTM A471 Class 13 Heat-Treated general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Chromium Molybdenum Steel

ASTM A471 Class 13 Heat-Treated thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K Typical for Chromium Molybdenum Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Chromium Molybdenum Steel
Specific heat capacity 23.0 °C Specific heat capacity of 448 - 502 J/(kg·K) Typical for Chromium Molybdenum Steel
Thermal conductivity 23.0 °C Thermal conductivity of 36 - 43 W/(m·K) Typical for Chromium Molybdenum Steel

ASTM A471 Class 13 Heat-Treated mechanical

Property Temperature Value Comment
Charpy impact energy 23.0 °C Charpy impact energy of 20 J -
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Chromium Molybdenum Steel
Elongation A50 23.0 °C Elongation A50 of 16 % -
Hardness, Brinell 23.0 °C Hardness, Brinell of 255 - 302 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Chromium Molybdenum Steel
Reduction of area 23.0 °C Reduction of area of 45 % -
Tensile strength 23.0 °C Tensile strength of 860 MPa -
Yield strength Rp0.02 23.0 °C Yield strength Rp0.02 of 725 - 860 MPa -