ASTM A471 Class 11 Heat-Treated
Equivalent material: ASTM Class 12, ASTM Class 13
ASTM A471 Class 11 Heat-Treated general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Molybdenum Steel |
ASTM A471 Class 11 Heat-Treated thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K |
Typical for Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 502 J/(kg·K) |
Typical for Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 36 - 43 W/(m·K) |
Typical for Chromium Molybdenum Steel |
ASTM A471 Class 11 Heat-Treated chemical
Property |
Value |
Aluminium |
Aluminium of 0.015 % |
Carbon |
Carbon of 0.38 - 0.43 % |
Chromium |
Chromium of 0.8 - 1.1 % |
Manganese |
Manganese of 0.6 - 1 % |
Molybdenum |
Molybdenum of 0.15 % |
Nickel |
Nickel of 0.5 % |
Phosphorus |
Phosphorus of 0.01 % |
Sulfur |
Sulfur of 0.015 % |
Vanadium |
Vanadium of 0.06 % |
ASTM A471 Class 11 Heat-Treated mechanical
Property |
Temperature |
Value |
Comment |
Charpy impact energy |
23.0 °C |
Charpy impact energy of 20 J |
- |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Molybdenum Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 20 % |
- |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 207 - 255 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Molybdenum Steel |
Reduction of area |
23.0 °C |
Reduction of area of 50 % |
- |
Tensile strength |
23.0 °C |
Tensile strength of 690 MPa |
- |
Yield strength Rp0.02 |
23.0 °C |
Yield strength Rp0.02 of 515 - 655 MPa |
- |