ASTM A426 Grade CP11 Austenitized and Tempered
Equivalent material: DIN 1.7338, DIN 1, 7357, EN 1.7338, EN 1, ASTM CP11, UNS J12072
ASTM A426 Grade CP11 Austenitized and Tempered general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Nickel Chromium Molybdenum Steel |
ASTM A426 Grade CP11 Austenitized and Tempered thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K |
Typical for Nickel Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Nickel Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 670 J/(kg·K) |
Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 34 - 54 W/(m·K) |
Typical for Nickel Chromium Molybdenum Steel |
ASTM A426 Grade CP11 Austenitized and Tempered chemical
Property |
Value |
Carbon |
Carbon of 0.05 - 0.2 % |
Chromium |
Chromium of 1 - 1.5 % |
Manganese |
Manganese of 0.3 - 0.8 % |
Molybdenum |
Molybdenum of 0.44 - 0.65 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.6 % |
Sulfur |
Sulfur of 0.025 % |
ASTM A426 Grade CP11 Austenitized and Tempered mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Chromium Molybdenum Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 20 % |
- |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 201 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Chromium Molybdenum Steel |
Reduction of area |
23.0 °C |
Reduction of area of 35 % |
- |
Tensile strength |
23.0 °C |
Tensile strength of 485 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 275 MPa |
- |
Choose our top-tier steel products to elevate the quality and strength of your structures and equipment.
-- Our promise
Similar or equivalent steel materials