ASTM A322 Grade 4037
Equivalent material: AISI 4037, SAE 4037, UNS G40370
ASTM A322 Grade 4037 general
| Property |
Temperature |
Value |
Comment |
| Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Molybdenum Steel |
ASTM A322 Grade 4037 thermal
| Property |
Temperature |
Value |
Comment |
| Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.29E-5 1/K |
Typical for Molybdenum Steel |
| Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Molybdenum Steel |
| Specific heat capacity |
23.0 °C |
Specific heat capacity of 456 J/(kg·K) |
Typical for Molybdenum Steel |
| Thermal conductivity |
23.0 °C |
Thermal conductivity of 37 - 48 W/(m·K) |
Typical for Molybdenum Steel |
ASTM A322 Grade 4037 chemical
| Property |
Value |
| Carbon |
Carbon of 0.35 - 0.4 % |
| Chromium |
Chromium of 0.2 % |
| Copper |
Copper of 0.35 % |
| Manganese |
Manganese of 0.7 - 0.9 % |
| Molybdenum |
Molybdenum of 0.2 - 0.3 % |
| Nickel |
Nickel of 0.25 % |
| Phosphorus |
Phosphorus of 0.04 % |
| Silicon |
Silicon of 0.15 - 0.35 % |
| Sulfur |
Sulfur of 0.04 % |
ASTM A322 Grade 4037 mechanical
| Property |
Temperature |
Value |
Comment |
| Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Molybdenum Steel |
| Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Molybdenum Steel |