ASTM A320 Grade L7A Quenched and Tempered
Equivalent material: AISI 4037, SAE 4037, ASTM Grade L71
ASTM A320 Grade L7A Quenched and Tempered general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Molybdenum Steel |
ASTM A320 Grade L7A Quenched and Tempered thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K |
Typical for Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 502 J/(kg·K) |
Typical for Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 36 - 43 W/(m·K) |
Typical for Chromium Molybdenum Steel |
ASTM A320 Grade L7A Quenched and Tempered chemical
Property |
Value |
Carbon |
Carbon of 0.35 - 0.4 % |
Manganese |
Manganese of 0.7 - 0.9 % |
Molybdenum |
Molybdenum of 0.2 - 0.3 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.15 - 0.35 % |
Sulfur |
Sulfur of 0.04 % |
ASTM A320 Grade L7A Quenched and Tempered mechanical
Property |
Temperature |
Value |
Comment |
Charpy impact energy |
23.0 °C |
Charpy impact energy of 27 J |
- |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Chromium Molybdenum Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 16 % |
- |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 321 [-] |
- |
Hardness, Rockwell C |
23.0 °C |
Hardness, Rockwell C of 35 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Molybdenum Steel |
Reduction of area |
23.0 °C |
Reduction of area of 50 % |
- |
Tensile strength |
23.0 °C |
Tensile strength of 860 MPa |
- |
Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 725 MPa |
- |
Tailor-made steel solutions to meet your unique requirements.
-- Our promise
Similar or equivalent steel materials